Resistance of a Wire Simulation

A wire taped to a metre rule, with a crocodile clip you slide along it. Digital meters give V and I with small, repeatable scatter, each reading drops onto an R–L graph with a best-fit line and gradient triangle, and a heating model shows why the current must stay small.

Loading simulation…
Show symbols for

Predict first

Question 1 of 4

With the crocodile clip at 25 cm, the meters give a resistance of about 1.1 Ω for the constantan wire. The clip is slid along to 50 cm and the wire stays cool. What resistance will the new reading give?

Try this

  1. 1Press Switch on, read the ammeter and the voltmeter, then press Record and Switch off. Drag the black crocodile clip (or use the Crocodile clip at slider) to 20 cm, and repeat at 40, 60, 80 and 100 cm.
  2. 2Record each length a second time and look at the Mean R column. Then read the Line of best fit box: does the line pass through the origin, and is the gradient close to 4.32 Ω per metre for 0.38 mm constantan?
  3. 3Press the 0.38 mm button under the stage until it shows 0.19 mm, then record the same lengths. Compare the gradients in the table under the graph: how many times steeper is the thinner wire's line?
  4. 4Choose Nichrome, move the clip to 10 cm, press Switch on and leave it on. Watch the Wire temperature card and the ammeter for half a minute, then switch off and try the same with constantan.
  5. 5Switch on Contact resistance at the clips and record the same five lengths again. Where does the new line meet the resistance axis, and has its gradient changed?

The bench

A thin wire lies along a wooden metre rule, taped down at each end. A red clip holds it at the zero mark and a black crocodile clip bites onto it wherever you put it, so the reading at that clip is the length of wire carrying current. The supply, an ammeter and that length of wire make a single series loop. The voltmeter is clipped on at those same two points, so its reading is the potential difference across only the stretch being tested. Both meters are digital and choose their own range, showing three decimal places below 2.

Two readings, one resistance

Each press of Record stores both meter readings and works out

R=VIR = \frac{V}{I}

The clip goes on afresh for the next reading, so a repeat at the same mark lands a millimetre or so away and gives a slightly different value. Two or three readings at every length, averaged, smooth out that scatter.

A straight line through zero

Plot the mean resistance against length and the crosses settle on a straight line aimed back at the origin. Twice the length gives twice the resistance, so R∝LR \propto L while the temperature holds steady. The gradient is the resistance of one metre of this wire. The dashed triangle under the line covers more than half of it, as examiners expect, and the box beneath the graph shows the division.

Thinner wire, steeper line

Resistance also depends on cross-sectional area, and the area of a round wire grows with the square of its diameter:

A=πd24A = \frac{\pi d^2}{4}

Half the diameter leaves a quarter of the area and four times the resistance per metre, so that line climbs four times as steeply. The micrometer panel measures the diameter at three points along the wire. Use the mean, because a 1% slip in dd becomes a 2% slip in AA.

Resistivity

Courses that go further merge both effects into R=ρL/AR = \rho L/A, where the resistivity ρ\rho belongs to the material, not the shape. Multiply the gradient by the measured area to find ρ\rho in ohm metres. Typical values are about 4.9×10−74.9 \times 10^{-7} for constantan, 1.1×10−61.1 \times 10^{-6} for nichrome and 1.7×10−81.7 \times 10^{-8} for copper. Copper makes a poor test wire: a whole metre of it has well under an ohm, about as much as the leads and clips.

Keep it cool

Current warms the wire, and a warmer metal resists more. Leave the supply on with a short piece of nichrome and the ammeter reading creeps down; force far too much current through and the wire starts to glow. Constantan hardly changes, which is why schools like it, yet it still gets hot enough to burn a finger. A low supply setting, sensible lengths and switching off between readings protect your results. The temperatures shown come from a simple model.

Zero errors

Switch on contact resistance and every reading picks up roughly 0.3 Ω extra. The new line runs parallel to the old one but meets the resistance axis above zero. That is why the gradient, rather than any single value of R÷LR \div L, gives the trustworthy answer.

In your course

AQA GCSE uses this set-up for Required practical 3 and asks only for V=IRV = IR and the effect of length, so area and resistivity are marked beyond GCSE. Cambridge IGCSE adds the effect of cross-sectional area but stops short of resistivity. The Punjab Physics 10 book uses R=ρL/AR = \rho L/A in Chapter 16.

Equations

  • Potential difference, current and resistance

    V=IR

    potential difference = current × resistance

    Open calculator →

Check your understanding

7 questions

  1. 1.A voltmeter across a length of wire reads 1.20 V while the ammeter reads 0.400 A. What is the resistance of that length?
  2. 2.50 cm of a uniform wire has a resistance of 2.0 Ω. What is the resistance of 75 cm of the same wire at the same temperature?
  3. 3.Keeping the material and the temperature the same, which change to a wire makes its resistance four times bigger?
  4. 4.Why should the supply be switched off between readings in this practical?
  5. 5.Where should the voltmeter be connected to measure the resistance of the length of wire in use?
  6. 6.A graph of R against L is a straight line that crosses the R axis at +0.3 Ω instead of at zero. What is the most likely cause?
  7. 7.A constantan wire has a resistance of 4.4 Ω per metre and a cross-sectional area of 1.1 × 10⁻⁷ m². What is its resistivity? (Beyond GCSE and IGCSE.)